Coating of powders

Contact angle measurement for optimizing the success of surface chemical modification

When powders are mixed with liquids, wetting problems often occur together with the formation of lumps. Powders for dispersions are therefore often provided with a coating which matches the liquid. Important examples of this are coated powders for paints and compound melts. Our measuring instruments for measuring the contact angle on powders help in the specific development and quality control of coatings.

Typical powder-coating applications

Surface-energy modification of powder surfaces

The properties of powders are dominated by their surface free energy, as the surface is large compared with the volume. Lumps occur when the work of cohesion is greater than the work of adhesion, that is to say when contact with the same type of surface is preferred. With the coating, the surface free energy is approximated to the surface tension of the liquid. This balances the energetic advantage of the interfacial contact for the two phases.

With the Washburn method of contact angle measurement, our Force Tensiometer – K100 provides a sound method of determining the surface free energy. In doing so, the rate of increase and the increase in mass of different liquids in a powder bulk in an immersed tube are measured. The better the powder wetting, the faster the liquid rises.

In the case of non-wettable powders, the contact angle is measured optically using our Drop Shape Analyzer based on drops dispensed on a powder bed.

Measuring polarity for the specific development of coatings

When different test liquids with known surface tension and polarity are used, as well as the surface free energy of the powder, our software also measures their polar and non-polar (dispersive) fractions. With the help of this information, the coating can be precisely adjusted to the polarity of the liquid in order to maximize the stability of the dispersion. Such preliminary investigations save many elaborate mixing tests on a semi-commercial scale, particularly in the development of compound plastics.

KRÜSS Application Reports

AR224: Dispersibility predictions - Some practical examples

The free surface energy of differently coated carbon black particles and different plastics is measured. The degree of mixability in the melt is predicted in each case based on calculated adsorption enthalpies and confirmed by stirring tests.